PTM 7000-SP | Phase Change Paste
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 0.06 Thermal Impedance
- 6.5 Thermal Conductivity
- Paste form
Product Description
PTM7000-SP is a viscous, stencil printable paste version of PTM7000. It is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. As with all Phase change materials, it has stable Thermal Impedance across accelerated aging tests and does not display bleed, pump or flow out. PTM7XXX product line has the highest Thermal conductivity and lowest thermal impedance out of the entire PTM Series.
PTM7000-SP has a Thermal conductivity of 6.5 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. This proprietary material has a maximum particle size of 50um, provides superior reliability and maintains low thermal impedance (0.06) , making it desirable for high-performance integrated circuit devices.
Please keep in mind that 7XXX is a Product Series. Base 7000 performs on the baseline of the stated properties while PTM7900 and PTM7950 are the highest performing materials of this product line reaching 8.5 W/m·K and 0.04 TI.
Solvent Drying time:
- 2.5 hours @ 23°C
- 2.5mins @ 100°C
Packaging
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Physical Properties
Additional Information
Accelerated Solvent Drying at 100°C
PTM7000-SP features a solvent system designed for efficient solvent evaporation following material application. For manufacturing processes requiring shorter drying times, elevated-temperature drying at 100°C can significantly accelerate solvent removal compared with ambient drying conditions.
As illustrated in the drying curve, PTM7000-SP exhibits rapid solvent evaporation at 100°C, reaching approximately 5.7% weight loss within the first 10 minutes. The weight loss gradually increases to approximately 6.3% after 30 minutes and approaches 6.7% after 120 minutes.
The rapid initial weight loss indicates that a substantial portion of the volatile components can be removed during the early stages of heating, making elevated-temperature drying a potential option for production processes requiring shorter drying cycles.
The drying profile at 100°C provides a useful reference for establishing drying parameters. However, the optimum drying duration should be validated based on the applied material thickness, drying equipment, airflow, and assembly requirements.
When choosing a printable paste it is important to understand the process parameters and limitations.
That's why we ask, when you contact us, to include the following information:
- What is your print thickness?
- How long is your printing time and working window?
- What is your drying step after printing?
- Temperature (Room temperature or something else?)
- Time
- Do you have any viscosity limitations in the printing process?

PTM7XXX Series - Pressure vs Thermal Impedance
PTM7XXX Series vs Competition comparison
What is the shelf-life of the PTM7000-SP?
Shelf-life refers to the amount of time the material can be kept when stored under the recommended storage conditions. The shelf-life of the PTM7000-SP is 12 months when kept below 25°C and with less than 20% relative humidity (RH).
How is the material prepared prior to use?
If the material is supplied in 280cc cartridges, then the PTM7000-SP can be dispensed directly onto the stencil. If the PTM7000-SP is supplied in 1kg can, then it is best to mix or roll the material prior to each use. "Rolling" involves simply having the material "self-mix" which the can is being rolled (for this there is standard "jar roller" equipment).
Any recommended printing equipment, squeegees etc?
DEK TQ stencil printers, currently made by ASM Pacific have been proven to work well. DEK equipment has built-in stencil cleaners. ASM also has recommended consumables to be used for printing. Rubber squeegee blades need to be cleaned every hour if they are not used continuously.
How should I transfer it to the dispensing tanks?
This question usually arises from customers that wonder whether to pour or pump the material. Our current customers are all pouring PTM7000 into the dispense tanks.
Which packaging, the 1kg can or the 280cc aluminum cartridge is best recommended to use?
This depends on how you plan to apply the material. If you plan to dispense from a cartridge (hardly anyone dispenses) using a nozzle, then a cartridge is recommended. Also, if you plan to do much smaller batch sizes (ie less then 1kg at a time), then 280cc cartridges are better because you will lose less material per use. Printing, however, is a high throughput process. On any print cycle you will need at least 100cc of material on the stencil during printing which can coat many pieces per stroke. You will easily use up 280cc of material per shift during printing.
What is the potlife of the PTM7000-SP?
Potlife (also referred to as work life) refers to the amount of time the material can be still be used after it has been opened. When kept in the 1kg cans, the potlife is 12 hours from the time the can is opened. When the lid is replaced and the can is closed again, you will have 48 hours to use the balance of the material. The remaining material should also be remixed (or re-rolled on a jar roller) prior to use.
Similarly, in the 280cc cartridge, the potlife is 24hrs if dispensed from the cartridge directly. If the cartridge is opened to add material to the printer and then closed again, the balance of the material should be used within 24-36 hours.
The work life of this phase change paste is 1 hour at room temperature, for the material that has been poured into the printer. If the solvents are allowed to evaporate for more than that, you won't be able to properly print. That's a sign that the material has gone bad. Please note that the material is optimized for printing and not for dispensing.
What is the thickness difference before and after drying?
It is typical to lose approx. 20% thickness due to solvent drying. For example, a 300µm (0.3mm) thickness stencil of wet PTM7000-SP will result in 240µm (0.24mm) after drying. If the thickness loss is more than 20%, then the can was not stirred or rolled and it is indicative of mixing issues prior to dispensing them on the printing equipment.
What is Homogeneity?
Homogeneity is caused by filler settling down during long periods of storage, if refrigerated, filler settling is much slower as compared to storing at room temperature. Refrigerated material should be thawed for 4hours before using.