MOLYKOTE L-2132

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

MOLYKOTE L-2132

Main features

  • High-Viscosity Enclosed-Gear Lubrication
  • Corrosion-Inhibited EP Formulation
  • Severe-Condition Micropitting Protection

Product Description

MOLYKOTE L-2132 Synthetic Gear Oil is a fully synthetic ISO VG 320 PAO gear oil for industrial gear units requiring extreme-pressure lubrication. Typical kinematic viscosity is 320 cSt at 40 deg C and 33.0 cSt at 100 deg C, with a viscosity index of 123 and a pour point below -37 deg C. Its sulfur-phosphorous EP additive and corrosion inhibitor support demanding spur, helical, bevel, and planetary gear service. This high-viscosity grade has a greater-than-12 FZG failure load stage and a 40/40/0 demulsibility result.

Key features

  • High-Viscosity Gear Coverage: The ISO VG 320 profile supports enclosed gear units requiring a higher-viscosity EP oil.
  • EP and Corrosion Additives: Sulfur-phosphorous EP chemistry and corrosion inhibition support demanding gear service.
  • Load and Water Separation: Typical results combine greater than 12 FZG stage with 40/40/0 demulsibility at 10 minutes.

Applications

Enclosed industrial spur, helical, bevel and planetary gear drives where the specified viscosity grade is required.

Product Family

MOLYKOTE L-2132

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density
Volumetric mass per unit
0.855 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
227 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values; not for use in preparing specifications.

PropertyValueUnitMethod / condition
ISO viscosity grade320-Manufacturer designation
Kinematic viscosity320cStASTM D445 at 40 deg C
Kinematic viscosity33.0cStASTM D445 at 100 deg C
Viscosity index123-ASTM D2270
Pour pointLess than -37deg CASTM D97
Water contentLess than 500ppmISO 3733
Demulsibility40/40/0mL/mL/mLASTM D1401; 10 min
FZG failure load stageGreater than 12-DIN 51354-2; A/8.3/90