MOLYKOTE L-2115
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Extreme-Pressure Enclosed-Gear Lubrication
- Micropitting-Focused PAO Protection
- Rapid 10-Minute Water Separation
Product Description
MOLYKOTE L-2115 Synthetic Gear Oil is a fully synthetic ISO VG 150 PAO gear oil for industrial gear units requiring an extreme-pressure lubricant. Typical kinematic viscosity is 162 cSt at 40 deg C and 18.2 cSt at 100 deg C, with a viscosity index of 128. The formulation combines a sulfur-phosphorous EP additive with corrosion inhibition and is designed for spur, helical, bevel, and planetary gears, including severe conditions where micropitting is a concern. Water separation is assessed by ASTM D1401 demulsibility testing, and load performance by FZG load-stage testing, for demanding enclosed-gear service.
Key features
- ISO VG 150 Gear Protection: The PAO grade combines sulfur-phosphorous EP additives with corrosion inhibition.
- Micropitting-Focused Formulation: The synthetic gear oil is designed for severe conditions where micropitting is a concern.
- Load and Water Separation: Typical results include greater than 12 FZG load stage and 40/40/0 demulsibility at 10 minutes.
Applications
Enclosed industrial spur, helical, bevel and planetary gear drives where the specified viscosity grade is required.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical values; not for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| ISO viscosity grade | 150 | - | Manufacturer designation |
| Kinematic viscosity | 162 | cSt | ASTM D445 at 40 deg C |
| Kinematic viscosity | 18.2 | cSt | ASTM D445 at 100 deg C |
| Viscosity index | 128 | - | ASTM D2270 |
| Pour point | Less than -43 | deg C | ASTM D97 |
| Water content | Less than 500 | ppm | ISO 3733 |
| Demulsibility | 40/40/0 | mL/mL/mL | ASTM D1401; 10 min |
| FZG failure load stage | Greater than 12 | - | DIN 51354-2; A/8.3/90 |