HUMISEAL 2UV11
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- UV-Gelled Shadow-Area Encapsulation
- Fast 15-Minute Handling
- Soft Shore A30 Encapsulation
Product Description
HumiSeal 2UV11 combines UV gelation with a secondary two-component reaction for shadowed areas in electronic potting and encapsulation. The 1:1 urethane/acrylate system pairs typical viscosities of 8,000 cP for Part A and 7,000 cP for Part B. It gels with UV exposure or after 7 minutes in shadow and reaches handling condition in 15 minutes. Typical full cure is 24 hours at room temperature, with cure time dependent on volume or mix ratio. The cured clear encapsulant has a soft Shore A30 hardness and a typical operating-temperature range of -50 to 110 deg C.
Key features
- UV gelation: The system gels with UV exposure.
- Shadow-area reaction: A secondary two-component reaction continues cure in shadowed areas.
- Soft cured material: The clear cured encapsulant has Shore A30 hardness.
Applications
Potting and encapsulation of electronic components.
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Values are typical product-selection data and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 8,000 | cP | Part A; typical |
| Viscosity | 7,000 | cP | Part B; typical |
| Mix ratio | 1:1 | Part A:Part B; basis not stated | |
| Gel response | UV exposure or 7 min in shadow | Typical | |
| Handling time | 15 | min | Typical |
| Full cure | 24 | h | Room temperature; typical; cure time may vary with volume or mix ratio |
After-processing / final-state properties
Values describe the cured material and are typical product-selection data, not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Clear | Cured material | |
| Hardness | A30 | Shore A | Cured material; typical |
| Operating temperature | -50 to 110 | deg C | Cured material; typical range |