HUMISEAL 2E10-B
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- Extended 60-Minute Pot Life
- Simple 1:1 System Mixing
- High Dielectric Strength Encapsulation
Product Description
HumiSeal 2E10-B is a two-component epoxy potting compound for industrial and electronic sealing, bonding, and encapsulation. The 1:1 system combines typical viscosities of 6,000 cP for Part A and 12,000 cP for Part B, with a 60-minute pot life and 180-minute handling time based on a typical 100 g volume. After cure, the black epoxy has Shore D85 hardness, a typical operating-temperature range of -50 to 125 deg C, and dielectric strength of 550 V/mil. Its equal-part mixing and extended work life suit controlled preparation of electronic and industrial potting assemblies.
Key features
- Equal-part preparation: A 1:1 ratio allows straightforward mixing of Part A and Part B.
- Extended pot life: Pot life is 60 minutes at a typical 100 g mixed volume.
- Dielectric strength: The cured epoxy has a typical dielectric strength of 550 V/mil.
Applications
Industrial sealing, bonding, and encapsulation.
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Values are typical product-selection data and are not specifications. Pot-life and handling-time values use a typical 100 g volume.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 6,000 | cP | Part A; typical |
| Viscosity | 12,000 | cP | Part B; typical |
| Mix ratio | 1:1 | Part A:Part B; basis not stated | |
| Pot life | 60 | min | Typical 100 g mixed volume |
| Handling time | 180 | min | Typical 100 g mixed volume |
After-processing / final-state properties
Values describe the cured material and are typical product-selection data, not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Black | Cured material | |
| Hardness | D85 | Shore D | Cured material; typical |
| Operating temperature | -50 to 125 | deg C | Cured material; typical range |
| Dielectric strength | 550 | V/mil | Cured material; typical |