DYMAX 9014

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DYMAX 9014

Main features

  • UV Cure with Moisture Backup
  • Controlled Gel Encapsulation
  • Dual-Cure Mechanical Protection

Product Description

Dymax Dual-Cure 9014 UV/Moisture-Curing Encapsulant is a room-temperature-stable yellow translucent gel for protecting wire bonds and chip assemblies. UV light provides the primary cure in exposed areas, while ambient moisture completes cure in shadowed regions that light cannot reach. Its gel rheology supports controlled placement and application-thickness management before cure. The cured encapsulant is stated with hardness, tensile strength, elongation, and modulus data after the combined cure process. Applications include chip-on-board, chip-on-flex, chip-on-glass, and wire-bond encapsulation.

Key features

  • UV cure with moisture backup: Light provides primary cure while ambient moisture addresses shadowed areas.
  • Gel placement control: The yellow translucent gel supports localized dispensing and controlled application thickness.
  • Balanced cured mechanical profile: Final-state documentation covers hardness, tensile strength, elongation, and modulus after dual cure.

Applications / Suitable for

  • Chip-on-board encapsulation
  • Chip-on-flex and chip-on-glass encapsulation
  • Wire-bond encapsulation

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light Yellow Translucent Gel
Chemistry Type
Acrylated Urethane
Density (g)
1.02 g/cm3
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.5
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
18,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
63 %
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
9.70E+13 Ohms⋅cm
Chemical Properties
Water Absorption
0.6 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
51 °C
Other Properties
Storage Temperature
10 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Application and cure-system characteristics before full dual-cure completion.

Property Value Unit Method / condition
Appearance Yellow translucent As supplied
Physical form Gel encapsulant As supplied
Primary cure UV light Light-accessible areas
Secondary cure Ambient moisture Shadowed areas
Storage behavior Room-temperature stable Before use
Application control Maximum recommended thickness applies Per stated dispense and cure conditions
Technical properties

After-processing / final-state properties

Final-state characteristics after the combined UV and moisture cure process.

Property Value Unit Method / condition
Cure state UV plus moisture cured Combined cure process
Shadowed-area completion Moisture secondary cure Areas not reached by UV light
Mechanical data scope Hardness; tensile strength; elongation; modulus After dual-cure completion
Encapsulation role Protective chip and wire-bond coverage Final installed state
Final application boundary Assembly- and cure-specific Evaluate the actual geometry and cure access