DOWSIL HM-2510
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Immediate Green Strength
- Up to 15-Minute Open Time
- 121 deg C Hot-Melt Application
Product Description
DOWSIL HM-2510 Assembly Sealant is a moisture-curing 100% silicone reactive hot-melt sealant that develops instant green strength after dispensing. The material has up to 15 minutes of open time, up to 24 hours of pot life, and is compatible with standard hot-melt dispensing equipment. The 121 deg C application temperature works with this hot-melt process, while high room-temperature viscosity resists flow and reduces squeeze-out. After cure, typical tensile strength is 670 psi with 1900% elongation, and the service-temperature range is -50 to 150 deg C. It is designed for assembly sealing and bonding on common substrates.
Key features
- Immediate Green Strength: Hot-melt application develops handling strength before the subsequent neutral moisture cure.
- Up to 15-Minute Open Time: Pot life is also listed up to 24 hours for the hot-melt process.
- 1900% Cured Elongation: Typical cured tensile strength is 670 psi.
Applications
Assembly sealing and bonding on common substrates using hot-melt application followed by moisture cure.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
Mechanical Properties
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Water clear | - | CTM 0176; typical |
| Viscosity | 1100 | poise | 120 deg C; CTM 0719; typical |
| Nonvolatile content | >98.5 | % | CTM 0086; typical |
| Open time | 15 | min | CTM 0243; typical |
| Specific gravity | 1.07 | - | Uncured; CTM 0044; typical |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Durometer | 38 | Shore A | CTM 0099; typical |
| Tensile strength | 670 | psi | ASTM D412; typical |
| Elongation | 1900 | % | ASTM D412; typical |
| Modulus at 50% elongation | 80 | psi | ASTM D412; typical |
| Service temperature range | -50 to 150 | deg C | ASTM C711; typical |