BONDERITE L-MR 9103
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Clear-View Machining Dilution
- Oil-Rejecting Coolant Operation
- Low-Foam Ferrous Metalworking
Product Description
BONDERITE L-MR 9103 is a synthetic, oil-rejecting, water-soluble metal-removal fluid for light-duty machining and grinding of ferrous alloys. When diluted to its typical 5 to 10% concentration range, it forms a clear blue solution that aids visibility around machining components. The fluid is formulated for clean running, foam control, and rejection of tramp oil, with built-in bio-resistance for sump operation. Its use remains limited to ferrous-alloy processing, providing a focused coolant choice for light-duty machining and grinding lines.
Key features
- Oil-Rejecting Fluid: Rejects tramp oil while maintaining a clear working solution when properly diluted.
- Low-Foam Operation: The synthetic fluid is identified as a no-foam product for machining processes.
- Clear Diluted Solution: A 5% dilution remains clear and blue to aid component visibility.
Applications
Light-duty machining and grinding of ferrous alloys at a typical 5 to 10% concentration.