BONDERITE C-AK 9045-6
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Ready-to-Use Carbon Removal
- 40 to 60 deg C Operation
- Mechanically Agitated Tank Cleaning
Product Description
BONDERITE C-AK 9045-6 AERO is a water-based alkaline degreaser and carbon remover for parts cleaning. Supplied ready to use, it removes carbon deposits and difficult soils from aircraft-engine components without mixing or dilution. The cleaner operates from 40 to 60 deg C and is used in mechanically agitated immersion tanks, including Turbulators and ultrasonic systems. It contains no chlorinated hydrocarbons, phenols, or chromates and is safe on common engine alloys. Applications include engine blocks, pistons, carburetors, transmissions, brake assemblies, and jet-engine overhaul.
Key features
- Ready-to-use cleaner: Supplied as received with no mixing or dilution required.
- Carbon and soil removal: Removes carbon deposits and difficult soils from aircraft-engine components.
- Moderate-temperature operation: Used at 40 to 60 deg C in mechanically agitated immersion systems.
Applications
Carbon and soil removal from engine blocks, pistons, carburetors, transmissions, brake assemblies, and jet-engine overhaul parts.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Use concentration | As received | - | No mixing or dilution required |
| Operating temperature | 40 to 60 | deg C | Preferred range; do not exceed 60 deg C |
| Immersion time | 30 minutes to 2 hours | - | Depends on contaminants to be removed |
| VOC | 161 | g/L | Rule 11241 |
| VOC vapor pressure | <1 | mm Hg | Rule 11241 |
| Recommended storage temperature | -5 to 40 | deg C | Store in closed containers away from excessive heat or direct sunlight |
| Shelf life | 24 | months | Unopened original packaging |