BONDERITE C-AK 4215 NC-LT

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 4215 NC-LT

Main features

  • Low-Temperature Multi-Metal Cleaning
  • Fuel/Hydraulic Component Cleaning
  • Chromate-Free Low-Foam Noncorrosive Formulation

Product Description

BONDERITE® C-AK 4215 NC-LT is a white granular alkaline cleaner developed for low-temperature cleaning of ferrous and nonferrous alloys using spray, immersion, and ultrasonic processes. The formulation is designed for cleaning fuel and hydraulic components and for preparing metal surfaces prior to metal bonding. Its balanced blend of organic surface-active agents provides controlled low-foam operation while remaining readily soluble, readily rinsable, free of chromates, and free of harsh caustics.

Key Features

  • Low-temperature alkaline cleaner for spray, immersion, and ultrasonic cleaning.
  • Suitable for ferrous and nonferrous alloys, including aluminum, steel, copper, and plated metals.
  • Controlled low-foam formulation designed for severe agitation conditions.
  • Readily soluble and free-rinsing for efficient cleaning and post-rinse performance.
  • Chromate-free and free of harsh caustics.

Applications / Suitable for

  • Fuel component cleaning
  • Hydraulic component cleaning
  • Cleaning prior to metal bonding
  • Spray cleaning systems
  • Immersion cleaning systems
  • Ultrasonic cleaning systems
  • Cleaning ferrous and nonferrous alloys

Technical Specifications

Other Properties
Storage Temperature
−10 to 50°C °C
General Properties
Appearance
Appearance at room temperature.
White granular mix
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Not Published

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal Pretreatment — Supplier classification
Product Type Alkaline Cleaner — Supplier classification
Application Spray, Immersion, Ultrasonic — Supplier classification
Appearance White granular mix — As supplied
Water solubility Readily soluble — Supplier feature
Foam characteristics Low foaming — Recommended concentrations and temperatures
Corrosion characteristics Noncorrosive to aluminum, steel, copper and plated metals — Supplier feature
Chromate content Chromate-free — Supplier feature
Storage temperature -10 to 50 °C Recommended storage
Technical Properties

After-Processing / Operating Properties

Property Value Unit Method / Condition
Spray concentration 7–15 g/L Spray cleaning
Spray operating temperature 45–55 °C 2–4 minutes
Spray cleaning time 2–4 minutes Supplier recommendation
Immersion concentration 45–60 g/L Air or mechanical agitation recommended
Immersion operating temperature 45–55 °C 5–10 minutes
Immersion cleaning time 5–10 minutes Supplier recommendation
Ultrasonic concentration 45–60 g/L Degas system before cleaning
Bath control Total alkalinity titration to pH 4.0 — 1 N sulfuric acid with Bromcresol Green indicator
Bath maintenance Maintain recommended concentration by adding fresh material — Supplier recommendation
Rinsing Cold to warm water — Spray or overflowing immersion rinse

Leading Brands Trust in Our Products and Services