AXAREL 56

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

AXAREL 56

Main features

  • Water-Rinsible Heavy-Soil Cleaning
  • Heated-Immersion Process Fit
  • Buffing-Compound and Grease Removal

Product Description

AXAREL 56 Solvent Cleaner uses highly refined solvents and surfactants in a water-rinsible formulation for heated immersion processing. It targets difficult soils that demand elevated-temperature cleaning, including buffing compounds, heavy greases, and other high-melting residues. The solvent-and-surfactant system combines strong soil removal with a water-rinse process step, making it relevant to precision-cleaning operations where residue removal follows heated soak treatment. Its supported uses include commercial and general aviation cleaning, precision cleaning, and heated immersion cleaning.

Key features

  • Water-rinsible formulation: Refined solvents and surfactants fit cleaning processes that include a water rinse.
  • Heated immersion use: Formulated for elevated-temperature soak cleaning.
  • Heavy-soil removal: Targets buffing compounds, heavy greases, and high-melting residues.

Applications

Applications include commercial and general aviation cleaning, precision cleaning, and heated immersion cleaning.

Product Family

AXAREL 56

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
96 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.84
Vapor Pressure
0.1 mmHg
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2.9 mPa.s